Warm red-brown. Deepens beautifully with age and finish.

Cherry grain study
Janka hardnessModerate

950 lbf

Softer than oak, and it marks. On cherry that is half the appeal — the patina is the reason people spec it.

Cost indexPremium

166 · red oak = 100

Indicative of lumber market position — not a UWP quote.

Availability

Milled to order · lead time confirmed at quote

Milled and finished at the Tanner Rd mill, NW Houston. Every wood stair part is special order.

What we mill it into

Character

Smooth, rich, and classic.

Softer than oak, and it marks. On cherry that is half the appeal — the patina is the reason people spec it.

Best for

Furniture-grade millwork and refined trim.

How Cherry behaves in service

Every board moves with the seasons, and in Houston the swing from a humid summer to a heated winter is the widest a floor or a tread will see. The figures below are the published shrinkage constants; the movement calculator turns them into inches for a given width.

Tangential shrinkageModerate movement

7.1%

Across a flatsawn face, green to oven-dry. The larger of the two and the one a wide plank follows.

Radial shrinkage

3.7%

Across a quartersawn face. Rift and quartered stock moves this much, which is why it is the stable cut.

Basis

USDA Wood Handbook

Published laboratory constants for the species, not a UWP measurement.

Finishing

Darkens from salmon to deep red-brown in its first year under light, so it is finished clear or with a light dye rather than a heavy stain. Blotches under pigment stain without a conditioner.

Machining and fastening

Machines like a dream: fine, even grain, little tear-out, a glassy surface off the planer. Burns on a slow cut. Holds fasteners well.

Closest in hardness

The three species nearest Cherry on the Janka scale — the usual alternatives when a budget, a tone or a lead time rules it out.