Jatoba — hardwood for stair treads and millwork

Deep reddish brown. Use when the design calls for a darker red hardwood.

Jatoba grain study
Janka hardnessVery hard

2,350 lbf

Nearly double red oak, and the hardest wood on this page by a wide margin. Pre-drill everything.

Cost indexFeature

214 · red oak = 100

Indicative of lumber market position — not a UWP quote.

Availability

Milled to order · lead time confirmed at quote

Milled and finished at the Tanner Rd mill, NW Houston. Every wood stair part is special order.

What we mill it into

Character

Dense, rich, and dramatic.

Nearly double red oak, and the hardest wood on this page by a wide margin. Pre-drill everything.

Best for

Premium accents and durable specialty work.

How Jatoba behaves in service

Every board moves with the seasons, and in Houston the swing from a humid summer to a heated winter is the widest a floor or a tread will see. The figures below are the published shrinkage constants; the movement calculator turns them into inches for a given width.

Tangential shrinkageModerate movement

8.5%

Across a flatsawn face, green to oven-dry. The larger of the two and the one a wide plank follows.

Radial shrinkage

4.5%

Across a quartersawn face. Rift and quartered stock moves this much, which is why it is the stable cut.

Basis

USDA Wood Handbook

Published laboratory constants for the species, not a UWP measurement.

Finishing

Deep orange-brown darkening to red under light; finished clear. Its density means a stain barely penetrates and an oil finish sits on the surface.

Machining and fastening

Very hard and heavy: it needs carbide tooling, pre-drilled fasteners and a slow feed, and it will burn. Interlocked grain tears out on the plane.

Closest in hardness

The three species nearest Jatoba on the Janka scale — the usual alternatives when a budget, a tone or a lead time rules it out.