Wood & material

Tearout

Fibres lifted and broken out of a surface by a cutter travelling against the grain.

Tearout happens when the knife lifts fibres instead of severing them, leaving a torn patch that sanding cannot fully remove because the damage runs below the surface.

It is controlled by feed direction, cutter sharpness, and taking lighter passes — and by reading the grain before the board goes through, which is why figured stock is slower to run.